I'm using Papi and occasionally DOA if the mix has high(er) solids.
Typically everything pours very easily without DOA.

Edward

On Wed, Jan 18, 2017 at 7:19 AM, James Padfield <james.padfield@xxxxxxxxx>
wrote:

From: Edward Wranosky <edwardcw@xxxxxxxxx>
Date: Mon, 9 Jan 2017 12:39:08 -0700
Subject: [AR] Re: N2O hybrid record -- paraffin grain

I have also used PEVA quite a bit for wax based hybrids, as well as
melting
asphaltum into the wax.
The best combination I've found yet is of HTPB and powdered wax. The
HTPB
encapsuates the powdered wax, yet allows for the lower melting point.
The
wax greatly increases the surface area of the HTPB, allowing it have a
high
regression rate. You can add in metals to this as well.

Edward


Out of curiosity, which isocyanate are using to cure the HTPB?  Any
plasticiser?