[pure-silver] Re: More (Semi) Standing Around

  • From: <C.Breukel@xxxxxxx>
  • To: <pure-silver@xxxxxxxxxxxxx>
  • Date: Tue, 9 Feb 2021 10:52:51 +0000

On Semi stand, or EMA or whatever:

I experimented a bit with it (notes are at home, so by heart) I think I used 
PyrocatHD 1+1+500 for sure for 1 hour, with vigoures agitation for 2 minutes at 
the beginning, and then modest agitation every 15 minutes). On Fomapan 100 
there was a definitive adjacent effect, actually too much, so I abounded that 
film. I had some ancient EFKE PL100 film left, and that worked quite nice. It 
depends on the subject matter, but for architecture I was quite pleased.

Oh and the point is I used vertical tubes filled to the brim with developer, so 
in my hands keeping the flim vertical was not needed.

Best,

Cor