You are doing what I believe to be carrect by addinmg a layer of tearaway
It gives you better definition
Re the difficulty of the fusible mesh removal - Preheat the edges first and 
then peel back and trim
I also agree w using 2 l;ayes of mesh cross patterned for larger stitch counts 
12-15,000 or more 
We specifically used a low melt -280F on ours so as not to scorch nor shrink 
your fabric.

mediumsetting for 10  - 12 seconds
As alwayds - if anyone wants samples pls e-mail me off list

Fred

=========================================================== 