Do you think it's different films or different grain sizes? In other words,
will fine grain react differently to large grain, or is it just a different
reaction depending on emulsions regardless of grain size?
Regards
Ralph W. Lambrecht
On 2005-04-26 16:55, "Martin Jangowski" <martin@xxxxxxxxxxxx> wrote:
> It seems that different films give very different reactions to
> different development methods. I found no very obvious differences between
> continous movement and semi-stand methods for the Deltas and APX100, so I
> basically stopped worrying and run everything thru the ATL.
=============================================================================================================
To unsubscribe from this list, go to www.freelists.org and logon to your
account (the same e-mail address and password you set-up when you subscribed,)
and unsubscribe from there.
- Follow-Ups:
- [pure-silver] Re: Development modifications for higher sharpness
- From: Martin Jangowski
- [pure-silver] Re: Development modifications for higher sharpness
- From: Ryuji Suzuki
- References:
- [pure-silver] Re: Development modifications for higher sharpness
- From: Martin Jangowski
Other related posts:
- » [pure-silver] Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- » [pure-silver] Re: Development modifications for higher sharpness
- [pure-silver] Re: Development modifications for higher sharpness
- From: Martin Jangowski
- [pure-silver] Re: Development modifications for higher sharpness
- From: Ryuji Suzuki
- [pure-silver] Re: Development modifications for higher sharpness
- From: Martin Jangowski