- From: Scott McMorrow <scott@xxxxxxxxxxxxx>
- Date: Tue, 07 Sep 2004 12:14:12 -0400
Another correction.
SI-glass has slightly lower loss than normal S-glass used in most laminates.
should be
SI-glass has slightly lower loss than normal E-glass used in most laminates.
Scott McMorrow wrote:
> One correction,
>
> there is a slight advantage in dielectric loss of N4000-13 SI over
> 4000-13.
> N4000-13 SI - lossTangent = 0.008 - 0.010
> N4000-13 - loss Tangent = 0.009 - 0.012
>
> SI-glass has slightly lower loss than normal S-glass used in most
> laminates. However, this difference is minimal when compared to FR-4
> which has a loss tangent of around 0.02 or higher. The advantage of SI
> material is in its low Er, lower even than Rogers 4350B, and better
> dielectric uniformity.
>
--
Scott McMorrow
Teraspeed Consulting Group LLC
121 North River Drive
Narragansett, RI 02882
(401) 284-1827 Business
(401) 284-1840 Fax
(503) 750-6481 Cellular
http://www.teraspeed.com
Teraspeed is the registered service mark of
Teraspeed Consulting Group LLC
------------------------------------------------------------------
To unsubscribe from si-list:
si-list-request@xxxxxxxxxxxxx with 'unsubscribe' in the Subject field
or to administer your membership from a web page, go to:
http://www.freelists.org/webpage/si-list
For help:
si-list-request@xxxxxxxxxxxxx with 'help' in the Subject field
List FAQ wiki page is located at:
http://si-list.org/wiki/wiki.pl?Si-List_FAQ
List technical documents are available at:
http://www.si-list.org
List archives are viewable at:
http://www.freelists.org/archives/si-list
or at our remote archives:
http://groups.yahoo.com/group/si-list/messages
Old (prior to June 6, 2001) list archives are viewable at:
http://www.qsl.net/wb6tpu
|

|